HY216Wear-resistant and anti-corrosion repair glue
HY216 wear-resistant repair agent contains fine-grained ceramic beads, and the wear resistance is 48 times that of ordinary cast iron. The wear-resistant and anti-corrosion repair agent can be widely used in the repair and pre-protection coating of the worn parts of the pump, impeller, feeder and other parts of erosion and cavitation.
Product details
HY216 wear-resistant repair agent contains fine-grained ceramic beads, and the wear resistance is 48 times that of ordinary cast iron. The wear-resistant and anti-corrosion repair agent can be widely used in the repair and pre-protection coating of the worn parts of the pump, impeller, feeder and other parts of erosion and cavitation.
Instructions
1. Surface treatment: Grind and roughen the surface to be repaired to a depth of more than 1mm and then clean it with HY755 cleaning agent or acetone. The surface to be trimmed must be clean, free of water and oil.
2 Mixing: Weigh components A and B according to the specified weight ratio, and mix them thoroughly to make the color completely consistent.
3 Coating: Use a rubber knife to apply the matched steel repair agent to the surface to be repaired. You can apply a small amount first, press it repeatedly with a rubber knife, and then apply the remaining repair agent after fully infiltrating, leaving a margin for processing.
4. Curing: After curing at room temperature for 12 hours, all kinds of mechanical processing can be carried out. When the ambient temperature is lower than 15 ℃, the curing time can be appropriately extended. Holding at 80℃ for 3 hours can shorten the curing time and obtain better coating properties.
Product specifications: 500g/set, 12 sets/box.
Instructions
1. Surface treatment: Grind and roughen the surface to be repaired to a depth of more than 1mm and then clean it with HY755 cleaning agent or acetone. The surface to be trimmed must be clean, free of water and oil.
2 Mixing: Weigh components A and B according to the specified weight ratio, and mix them thoroughly to make the color completely consistent.
3 Coating: Use a rubber knife to apply the matched steel repair agent to the surface to be repaired. You can apply a small amount first, press it repeatedly with a rubber knife, and then apply the remaining repair agent after fully infiltrating, leaving a margin for processing.
4. Curing: After curing at room temperature for 12 hours, all kinds of mechanical processing can be carried out. When the ambient temperature is lower than 15 ℃, the curing time can be appropriately extended. Holding at 80℃ for 3 hours can shorten the curing time and obtain better coating properties.
Product specifications: 500g/set, 12 sets/box.